D. W. Gandy, G. Frederick, K. Coleman, EPRI, Charlotte, NC
Summary: Two separate welding technologies are being developed to address failures in heat recovery steam generator tubing. The first, addresses tubing failures that occur along the length of a tube. The second addresses failures that occur at stub tube-to-header attachment locations. Welding developments for each failure location are discussed.